Polymer Property : Compressive Strength = 2.51 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 2.51 MPa

@Temperature 375 °C
364 psi

@Temperature 707 °F
Pyrotek Wollite 30 Insulating Castable
Wollite material is a solid, light weight mineral foam which is stable during its preparation and during subsequent curing and drying. Because of the foam properties it is well suited for casting c..