Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 190 MPa | 27600 psi | ASTM D695 |
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Compressive Strength | 190 MPa | 27600 psi | ASTM D695 |
Premix Premi-Glas® 1200H-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Compressive Strength | 190 MPa | 27600 psi | ASTM D695 |
Premix Premi-Glas® 1240-25 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-25 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Compressive Strength | 190 MPa | 27500 psi | ASTM D695 |
PolyOne Edgetek® SF-30CF/000 Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Compressive Strength | >= 190 MPa | >= 27600 psi | |
Hybrid Plastics Fireban® Mark VI Resorcinolinic (PRF) The resin system produces a superiour fire resistant material.Information provided by Hybrid Plastics |
|||
Compressive Strength | >= 190 MPa | >= 27600 psi | |
Hybrid Plastics Fireban® Mark VII Resorcinolinic (PRF) The resin system produces a superiour fire resistant material.Information provided by Hybrid Plastics |
|||
Compressive Strength | >= 190 MPa | >= 27600 psi | |
Hybrid Plastics Fireban® Mark VII-IS Resorcinolinic (PRF) The resin system produces a superiour fire resistant material.Information provided by Hybrid Plastics |
|||
Compressive Strength | >= 190 MPa | >= 27600 psi | |
Hybrid Plastics Fireban® Mark VI-IS Resorcinolinic (PRF) The resin system produces a superiour fire resistant material.Information provided by Hybrid Plastics |
|||
Compressive Strength | 190 MPa | 27600 psi | ASTM D695 |
Sumitomo Bakelite North America EM 7302LD-2 Long Glass Fiber Reinforced Epoxy EM 7302LD-2 is a long fiberglass reinforced epoxy molding compound with a low density inert filler. This compound is designed for applications where moderate strength and weight savings are desirabl.. |
|||
Compressive Strength | >= 190 MPa | >= 27600 psi | |
Master Bond EP112M Two Component, Medium Viscosity Heat Curing Cycloaliphatic Epoxy Resin Product Description: Master Bond Polymer System EP112M is a solventless, medium viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor .. |
|||
Compressive Strength | 190 MPa | 27600 psi | ASTM D695 |
Plenco 2369 Phenolic, Granular, Transfer Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Compressive Strength | 190 MPa | 27600 psi | |
Cosmic Plastics CP7318 Short Glass Fiber Filled Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 190 - 280 MPa | 27600 - 40600 psi | |
Goodfellow Potassium Aluminosilicate (Muscovite Mica) Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin.. |
|||
Compressive Strength | 190 MPa | 27600 psi | ASTM D695 |
Plenco 2571 Phenolic, Granular, Injection Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Compressive Strength | 190 MPa | 27600 psi | ASTM D695 |
Plenco 4568 Phenolic, Granular, Compression Molded PLENCO 04568 is a heat resistant, mineral and flock filled, phenolic molding compound, formulated to provide thermal oxidation stability along with excellent dimensional stability. 04568 is availabl.. |
|||
Compressive Strength | 190 - 220 MPa | 27600 - 31900 psi | ISO 604 |
Vyncolit 2950 W Novolac Phenolic Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Compressive Strength | 190 MPa | 27600 psi | ISO 604 |
Vyncolit G865 Novolac Phenolic Glass fiber filled phenolic molding compound with high mechanical, good thermal and electrical properties. USES: Asbestos-free replacement for die-cast automotive metal parts, e.g. reactors for aut.. |
|||
Compressive Strength | 190 MPa | 27600 psi | |
BCC Products BC 7136-2 Epoxy Casting BC7136-2 is an aluminum filled thick section casting system with heat resistance to 300ºF. May be cast to a thickness of 2 inches in non-conductive molds, 3 inches in conductive molds and thicker s.. |
|||
Compressive Strength | 190 MPa | 27600 psi | ASTM D695 |
Sumitomo Bakelite North America Epiall® 1908M-1 Short Glass Fiber Reinforced Epoxy Epiall 1908M-1 is a short glass fiber reinforced epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information provided.. |
|||
Compressive Strength | 190 MPa | 27600 psi | ASTM D695 |
Sumitomo Bakelite North America RX® 853G Fiberglass Reinforced Phenolic Novolac RX 853G is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am.. |
|||
Compressive Strength | 190 MPa | 27600 psi | ASTM D695 |
Owens Corning Glass Fiber Reinforced Polyester, Woven Roving (Lay-up), 50 wt.% glass Data provided by the manufacturer, Owens Corning. |
|||
Compressive Strength | 190 MPa | 27600 psi | |
Cosmic Plastics CP7314 Epoxy Molding Compound Data provided by the manufacturer. |