Polymer Property : Compressive Strength = 189 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 189 MPa

@Thickness 13.0 mm
27400 psi

@Thickness 0.512 in
ASTM D695
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
Compressive Strength 189 MPa
27400 psi
ASTM D695
Sumitomo Bakelite Durez® 22257 Phenolic, Compression Grade
Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. ..
Compressive Strength 189 MPa
27400 psi
ASTM D695
Plenco 5488 Phenolic, Granular, Injection Molded
PLENCO 05488 is a woodflour and graphite filled phenolic molding compound offering improved abrasion resistance. UL recognized under component file E40654. 05488 is available in brown. 05488 is not ..
Compressive Strength 189 MPa
27400 psi
ASTM D695
Plenco 7476 Phenolic, Granular, Transfer Molded
PLENCO 07476 is a cotton flock filled resole phenolic molding compound, with improved physical strength, crack resistance, and is resistant to soap and detergent solutions at elevated temperatures. ..
Compressive Strength 189 MPa

@Thickness 13.0 mm
27400 psi

@Thickness 0.512 in
ASTM D695
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..