Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 183 MPa | 26500 psi | ASTM D695 |
Owens Corning Glass Fiber Reinforced Nylon 6/6, 30 wt.% glass Nylons, as a group, are inert to most organic solvents. They resist alkalis and salt solutions and they are attacked by strong mineral acids and oxidizing agents. Data provided by the manufacturer,.. |
|||
Compressive Strength | 183 MPa | 26500 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Compressive Strength | 183 MPa | 26500 psi | 10% Def.; ASTM D695 |
Quadrant EPP Semitron® 480 ESd PEEK, static dissipative, extruded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic ProductsThis PEEK based static dissipative material provides a dissipative range of 10E+6 - 10E+9 ohms/sq. Semitron® ESd 480 is very dimensionally sta.. |
|||
Compressive Strength | 183 MPa | 26500 psi | ASTM D695 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Compressive Strength | 183 MPa | 26500 psi | ASTM D695 |
Plenco 4466 Phenolic, Granular, Transfer Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Compressive Strength | 183 MPa | 26500 psi | ASTM D695 |
Plenco 4599 Phenolic, Granular, Injection Molded PLENCO 04599 is a mineral filled, phenolic molding compound offering excellent heat resistance and dimensional stability, typically required for automotive ashtray applications. 04599 is formulated .. |
|||
Compressive Strength | 183 MPa | 26500 psi | ASTM D695 |
Plenco 4504 Phenolic, Granular, Compression Molded Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c.. |
|||
Compressive Strength | 183 MPa | 26500 psi | ASTM D695 |
Plenco 4548 Phenolic, Granular, Injection Molded PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai.. |
|||
Compressive Strength | 183 MPa | 26600 psi | ASTM D695 |
Ensinger Tecapeek® XP-106 Compression Molded PEEK Compound, 40% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |