Mechanical Properties Metric English Comments
Compressive Strength 1790 MPa
260000 psi
55 HRC
Schmolz + Bickenbach Cryodur® 2363 (A-2) Cold Work Die Steel
Description: Cryodur® 2363 is a cold-work steel developed for an excellent combination of wear resistance and toughness and Supplied in the annealed conditionCharacteristics: Good wear resistance; ..