Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 172 MPa | 24900 psi | |
Poco Graphite SCF-2 Ion Implant Grade Graphite An economic alternative to DFP-3-2, this 5-micron material is harder than DFP-3-2 and has high strengths without reduced porosity. |
|||
Compressive Strength | 172 MPa | 24900 psi | |
Pyrotek TS-550 Insulating Board TS-550 is phenolic-based, fiber and mineral reinforced, high-temperature material. TS-550 offers the high strength and wear resistant properties of laminated materials, while also offering the form.. |
|||
Compressive Strength | 172 MPa | 25000 psi | 10% Deformation; ASTM D695 |
Quadrant EPP Duratron® PI D7015G PI Bearing Grade Polyimide (ASTM Product Data Sheet) |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
IDI Composites W-103 Thermoset Polyester, Molding Premium appearance grade materials in a range of strengths for cookware and appliance applications.Data provided by the manufacturer. |
|||
Compressive Strength | 172 MPa @Thickness 12.7 mm |
25000 psi @Thickness 0.500 in |
Flatwise |
Industrial Laminates/Norplex ES-1 Engraving Stock Description: Composed of white melamine paper core with various pigmented cover sheets.Thickness Tested: 0.0620â€, 0.125â€, and 0.500†|
|||
Compressive Strength | 172 MPa @Thickness 12.7 mm |
25000 psi @Thickness 0.500 in |
Flatwise |
Industrial Laminates/Norplex ES-2 Engraving Stock Description: Composed of black phenolic paper core, sub surfaces of white melamine, and various pigmented cover plies. |
|||
Compressive Strength | 172 MPa @Thickness 12.7 mm |
25000 psi @Thickness 0.500 in |
Flatwise |
Industrial Laminates/Norplex ES-3 Engraving Stock Description: Contains black phenolic/paper core and various colored covers impregnated with melamine resin. |
|||
Compressive Strength | 172 MPa @Thickness 12.7 mm |
25000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP101 Synthetic Fabric Description: Phenolic resin combined with spun nylon fabric. Good impact strength and excellent electrical properties under high humidity conditions. Meets applicable Boeing specification, but exemp.. |
|||
Compressive Strength | 172 MPa @Thickness 12.7 mm |
25000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP629 Paper Base Laminate Description: It is a paper-phenolic high-pressure laminate. It is intended primarily for mechanical applications and is suitable for electrical applications as well. Thickness Tested: 0.062", 0.125".. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications .. |
|||
Compressive Strength | 172 MPa | 25000 psi | ASTM D695 |
Techmer ES Electrafil® J-1/CF/30/TF/13/SI/2 Nylon 66, 30% Carbon Fiber, 13% PTFE, 2% Silicone |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Sumitomo Bakelite North America E 16521A Electrical Encapsulation Grade Epoxy E-16521A is an encapsulation grade epoxy molding compound suitable for electrical applications such as coils.Information provided by Sumitomo Bak North America, Inc. |
|||
Compressive Strength | 172 MPa | 24900 psi | |
Cosmic Plastics 6220 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 172 MPa | 24900 psi | |
Cosmic Plastics 6220F Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Plenco 6990 Phenolic, Briquette, Compression Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Plenco 4300 Phenolic, Granular, Transfer Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Compressive Strength | 172 MPa | 25000 psi | 10% Deformation; ASTM D695 |
Ensinger Tecapeek® XP-119 Compression Molded PEEK Compound, 10% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Compressive Strength | 172 MPa | 25000 psi | ASTM D695 |
Applied Composites 8041 Polyester SMC Industry Application: ElectricalProduct Application: Business MachinesDistinct Features: UL 94-VO, Radiant Panel |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Vyncolit INSUL-PLATE™ X-28057-2HT Hole-Fill Powder For Printed Circuit Boards Vyncolit INSUL-PLATE™ Hole-Fill material delivers true reliability and superior performance. This material, in powder form, is specifically suited for Hole-Fill use in glass epoxy, multi-layer and .. |
|||
Compressive Strength | 172 MPa | 25000 psi | Break; TM R050-38 |
Resinlab® EP1282 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |
|||
Compressive Strength | 172 MPa | 25000 psi | Ultimate; TM R050-38 |
Resinlab® EP1282 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |
|||
Compressive Strength | 172 MPa | 25000 psi | Break; TM R050-38 |
Resinlab® EP691 Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP691 is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting and ad.. |
|||
Compressive Strength | 172 MPa | 25000 psi | Ultimate; TM R050-38 |
Resinlab® EP691 Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP691 is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting and ad.. |
|||
Compressive Strength | 172 MPa | 25000 psi | Ultimate; TM R050-38 |
Resinlab® EP1115 Clear Unfilled Epoxy Adhesive Resinlab™ EP1115 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Compressive Strength | 172 MPa | 25000 psi | Ultimate; TM R050-38 |
Resinlab® EP1282 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |
|||
Compressive Strength | 172 MPa | 24900 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Conditioned
(discontinued **) Availability: Asia Pacific; Europe; North AmericaInformation provide by Solvay Specialty Polymers |