Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
IDI Composites 46-12 Thermoset Polyester, Molding Highest strength electrical grade with good track resistance and V-O flame resistance.Data provided by the manufacturer. |
|||
Compressive Strength | 159 MPa | 23000 psi | |
SGL Carbon Group EK 203 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 159 MPa | 23000 psi | |
SGL Carbon Group EK 2230 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
Plenco 3303 Phenolic, Granular, Compression Molded Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b.. |
|||
Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
Plenco 3356 Phenolic, Granular, Injection Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |
|||
Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
Plenco 3356 Phenolic, Granular, Transfer Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |
|||
Compressive Strength | 159 - 172 MPa | 23000 - 25000 psi | |
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit.. |
|||
Compressive Strength | 159 - 193 MPa | 23000 - 28000 psi | |
Bulk Molding Compounds BMC 695 Vinyl Ester Molding Compound BMC 695 vinyl ester molding compound is a mineral filled glass fiber-reinforced vinyl ester compound suitable for compression and injection molding It is characterized by good moldability, oil and s.. |
|||
Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret.. |
|||
Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
Resinoid 2016P Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Compressive Strength | 159 MPa | 23000 psi | Ultimate; TM R050-38 |
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go.. |
|||
Compressive Strength | 159 MPa | 23100 psi | ASTM D695 |
Resinoid 2020 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Compressive Strength | 159 MPa | 23100 psi | Conditioned; ASTM D695 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |