Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 138 MPa | 20000 psi | Ultimate; TM R050-38 |
Resinlab® EP1290 Clear Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Clear is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to .. |
|||
Compressive Strength | 138 MPa | 20000 psi | |
Pyrotek NT-C Electrical Insulating Material NT-C offers superior arc and heat resistance properties, with adequate strength properties to withstand mechanical stress and hold up in severe electrical insulating applications. NT-C does not pro.. |
|||
Compressive Strength | 138 MPa | 20000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Ketron® 1000 IM Injection Molded Unfilled Polyetheretherketone (ASTM Product Data Sheet) Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam |
|||
Compressive Strength | 138 MPa | 20000 psi | ASTM D695 |
PolyOne Edgetek® PF-20GF/000 Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Compressive Strength | 138 MPa | 20000 psi | Ultimate; TM R050-38 |
Resinlab® EP1385 Black Epoxy Formulation Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Compressive Strength | 138 MPa | 20000 psi | Break; TM R050-38 |
Resinlab® EP1385 Black Epoxy Formulation Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Compressive Strength | 138 MPa | 20000 psi | Ultimate; TM R050-38 |
Resinlab® EP1385 Clear Epoxy Formulation Resinlab™ EP1385 Clear is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Compressive Strength | 138 MPa | 20000 psi | |
Poco Graphite DFP-3-2 Ion Implant Grade Graphite This is a high strength graphite that has reduced porosity. DFP-3-2 has long been the standard for components that exhibit long life and reduced erosion rates. |
|||
Compressive Strength | 138 MPa | 20000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Duratron® PAI T4540 Polyamide-imide, compression molded (ASTM Product Data Sheet) |
|||
Compressive Strength | 138 MPa | 20000 psi | ASTM D695 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only.. |
|||
Compressive Strength | 138 MPa @Temperature 260 °C |
20000 psi @Temperature 500 °F |
|
Haysite Heatmeiser® H340 Platen Insulation Haysite’s family of mold and platen insulation products are specially engineered fiberglass reinforced thermoset polyester composites which offer superior energy efficiency, temperature control.. |
|||
Compressive Strength | 138 MPa | 20000 psi | ASTM D695 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI) Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not .. |
|||
Compressive Strength | 138 MPa | 20000 psi | ASTM D695 |
Techmer ES Plaslube® J-1/CF/10/TF/13/SI/2 BK223 PA66 |
|||
Compressive Strength | >= 138 MPa | >= 20000 psi | |
Master Bond EP112FLAN-1 Two Component Flexibilized Heat Curing Epoxy Master Bond EP112FLAN-1 is a toughened two component, high performance epoxy resin system featuring good temperature resistance, high thermal conductivity, fine electrical insulation values and soun.. |
|||
Compressive Strength | >= 138 MPa | >= 20000 psi | |
Master Bond EP112FLAO-1 Toughened, Two component, Heat Curing Epoxy Master Bond EP112FLAO-1 is a toughened two component, high performance epoxy resin system featuring very good temperature resistance, fine thermal conductivity and electrical insulation values with .. |
|||
Compressive Strength | >= 138 MPa | >= 20000 psi | |
Master Bond EP112LS Two part, heat curing epoxy for potting, encapsulation, coating, sealing and impregnation Master Bond EP112LS is a low viscosity two component epoxy resin system for potting, encapsulation, sealing, coating and impregnation. The mix ratio is an easy to use 100:80 by weight. EP112LS offer.. |
|||
Compressive Strength | >= 138 MPa | >= 20000 psi | |
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT is an one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation prof.. |
|||
Compressive Strength | >= 138 MPa | >= 20000 psi | |
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT-LO is a one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation pr.. |
|||
Compressive Strength | >= 138 MPa | >= 20000 psi | |
Master Bond EP30AOHT Dimensionally Stable, Two Component Epoxy Description: Master Bond Polymer System EP30AOHT is a two component epoxy resin system for high performance bonding, potting, sealing and coating, formulated to cure at room temperature or more rapi.. |
|||
Compressive Strength | >= 138 MPa | >= 20000 psi | |
Master Bond Ep46HT-2 Two Component, Heat Resistant Epoxy System Master Bond Polymer System EP46HT-2 is a two component epoxy system for bonding, sealing and casting applications where resistance to temperatures from -100°F to +500°F is required. It is 100% rea.. |
|||
Compressive Strength | 138 - 152 MPa | 20000 - 22000 psi | |
Bulk Molding Compounds BMC 1410 Electrical Grade BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally.. |
|||
Compressive Strength | 138 - 172 MPa | 20000 - 25000 psi | |
Bulk Molding Compounds BMC 6605A Polyester Molding Compound |
|||
Compressive Strength | 138 MPa | 20000 psi | ASTM D695 |
Quantum Nylon 6/6 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Strength | 138 MPa | 20000 psi | Break; TM R050-38 |
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |
|||
Compressive Strength | 138 MPa | 20000 psi | Break; TM R050-38 |
Resinlab® EP1238 Acrylic / Epoxy Hybrid Adhesive Resinlab™ EP1238 is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wetting to.. |
|||
Compressive Strength | 138 MPa | 20000 psi | |
Cosmic Plastics 3D36 Thermoset Polyester Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 138 MPa | 20000 psi | Break; TM R050-38 |
Resinlab® EP1199 Clear Unfilled Epoxy Adhesive Resinlab™ EP1199 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Compressive Strength | 138 MPa | 20000 psi | Ultimate; TM R050-38 |
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi.. |
|||
Compressive Strength | 138 MPa | 20000 psi | Break; TM R050-38 |
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go.. |
|||
Compressive Strength | 138 MPa | 20000 psi | Ultimate; TM R050-38 |
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel th.. |