Mechanical Properties Metric English Comments
Compressive Strength 136 MPa
19700 psi
ASTM D695
Plenco 08218 Polyester BMC, Compression Molded
PLENCO 08218 is a renumber of PlasGlas 20118. PLENCO 08218 is an 18% glass-filled polyester bulk molding compound characterized as an electrical grade, but has many outstanding properties that make ..
Compressive Strength 136 MPa
19700 psi
ASTM D695
Plenco 08225 Polyester BMC, Compression Molded
PLENCO 08225 is a renumber of PlasGlas 20215. PLENCO 08225 is a 15% glass-filled polyester bulk molding compound characterized as a medium strength electrical grade, but has many outstanding propert..
Compressive Strength 136 MPa
19700 psi
TriStar TriSteel PE Metal Backed PTFE Bearing System
Ultraflon 603 PE lined metal backed bearing system, with or without lube, high PV, high temperature... Ultraflon 603 PE Liner is a bearing grade polymer for use in lubricated or unlubricated environ..
Compressive Strength 136 MPa
19700 psi
Poco Graphite Glassmate® HT Graphite
This high strength material has an oxidation inhibitor that raises the oxidation threshold. Service temperature can be raised to 600°C; graphites are subject to oxidation above 450°C