Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 13.8 MPa | 2000 psi | Break; Mixed 1:2; TM R050-38 |
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature.. |
|||
Compressive Strength | 13.8 MPa | 2000 psi | Ultimate; Mixed 1:2; TM R050-38 |
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature.. |
|||
Compressive Strength | 13.8 MPa | 2000 psi | Maximum working pressure |
Potters Industries Q-Cel® 6042S Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Compressive Strength | <= 13.8 MPa | <= 2000 psi | Working pressure |
Potters Industries Q-Cel® 7040S Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Compressive Strength | 13.8 MPa | 2000 psi | Break; TM R050-38 |
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (.. |
|||
Compressive Strength | 13.8 MPa | 2000 psi | |
SPHERE ONE EXTENDOSPHERESâ„¢ 300/600 Hollow Spheres EXTENDOSPHERESâ„¢300/600 are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, they can .. |
|||
Compressive Strength | 13.8 - 27.6 MPa | 2000 - 4000 psi | Crush Strength |
Trelleborg Fillite® 160W Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Compressive Strength | 13.8 - 27.6 MPa | 2000 - 4000 psi | Crush Strength |
Trelleborg Fillite® SGHA (500HA) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Compressive Strength | 13.8 - 27.6 MPa | 2000 - 4000 psi | Crush Strength |
Trelleborg Fillite® 300W Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Compressive Strength | 13.8 - 103 MPa | 2000 - 15000 psi | |
Du-Co Ceramics S-461 Magnesia Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
Compressive Strength | 13.8 - 41.4 MPa | 2000 - 6000 psi | |
Du-Co Ceramics S-570 Silica Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
Compressive Strength | 13.8 MPa | 2000 psi | |
3M HGS2000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |
|||
Compressive Strength | 13.8 MPa | 2000 psi | |
3M S32 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Compressive Strength | 13.8 MPa | 2000 psi | |
Aremco Ceramacast™ 675 High Temperature Potting & Casting Material Aluminum Nitride Fine grain aluminum nitride castable with high thermal conductivity |
|||
Compressive Strength | 13.8 MPa | 2000 psi | |
Aremco Ceramacast™ 675-N High Temperature Potting & Casting Material Aluminum Nitride Fine grain aluminum nitride castable with high thermal conductivity. |
|||
Compressive Strength | 13.8 - 20.7 MPa | 2000 - 3000 psi | |
Abatron AboCast 7802-1/AboCure 50-3 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, .. |
|||
Compressive Strength | 13.8 - 20.7 MPa | 2000 - 3000 psi | |
Abatron AboCast 7802-1/AboCure 7804-4 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia.. |
|||
Compressive Strength | 13.8 - 20.7 MPa | 2000 - 3000 psi | ASTM D695 |
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Compressive Strength | >= 13.8 MPa | >= 2000 psi | ASTM C365 |
Touchstone CFOAM® 25 Structural Carbon Foam CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins.. |
|||
Compressive Strength | 13.8 MPa | 2000 psi | |
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru.. |