Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 125 MPa | 18100 psi | |
Poco Graphite EDM-3 EDM Graphite POCO's EDM-3 is an isotropic Ultrafine grain graphite which offers high strength with outstanding wear and fine surface finish characteristics easily machined to thicknesses of .005 or less.Applicat.. |
|||
Compressive Strength | 125 MPa | 18200 psi | 10% Def.; ASTM D695 |
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet) |
|||
Compressive Strength | 125 MPa | 18100 psi | ASTM D695, Cond. A |
Haysite Heatmeiser® H340 Platen Insulation Haysite’s family of mold and platen insulation products are specially engineered fiberglass reinforced thermoset polyester composites which offer superior energy efficiency, temperature control.. |
|||
Compressive Strength | 125 MPa | 18100 psi | ASTM D695 |
Plenco 08112 Polyester BMC, Compression Molded PLENCO 08112 is a renumber of PlasGlas 10112. PLENCO 08112 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |
|||
Compressive Strength | 125 MPa | 18100 psi | Absolute Drying; ASTM-D695 |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Compressive Strength | >= 125 MPa | >= 18100 psi | Axial; IEC 1212-2 4.2 |
Hippe EP CC 31 Woven Cotton Cloth Reinforced Epoxy Resin - Round, Molded Tube and Rod Used in mechanical, electrical and electronic applications.Information provided by Hippe. |