Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 110.3 MPa | 16000 psi | Parallel to pressing direction |
Momentive Performance Materials HBN Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Compressive Strength | 110.3 MPa | 16000 psi | |
Henkel Hysol EA 9377 Paste Adhesive System Moldable plastic shim, excellent microcracking resistance under thermal cycling. High compressive strength.Application: Liquid Shim |