Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 108 MPa | 15700 psi | 20% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Conditioned Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 108 MPa | 15700 psi | 20% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Dry Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 108 MPa @Time 36.0 sec |
15700 psi @Time 0.0100 hour |
|
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance.. |
|||
Compressive Strength | 108 MPa @Time 360000 sec |
15700 psi @Time 100 hour |
|
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |
|||
Compressive Strength | 108 MPa @Time 36.0 sec |
15700 psi @Time 0.0100 hour |
|
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |
|||
Compressive Strength | 108 MPa | 15600 psi | Cold Crushing Strength |
Chosun Refractories BTB-18SC Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 108 MPa | 15600 psi | Cold Crushing Strength |
Chosun Refractories SAL90N Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 108 MPa | 15600 psi | Cold Crushing Strength |
Chosun Refractories SAL90Z Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 108 MPa | 15600 psi | 10% deformation; ASTM D695 |
Beijing Ranger Chem BLUESTAR® BS450 Acetal Copolymer Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Compressive Strength | 108 MPa | 15700 psi | |
Abatron AboCast/AboCure 4-4/50-12 Casting Epoxy for Tooling Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: FastBest rigid, chemical, and hea.. |
|||
Compressive Strength | 108 MPa | 15600 psi | 10% deformation; ASTM D695 |
Beijing Ranger Chem BLUESTAR® BS350 Acetal Copolymer Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Compressive Strength | 108 MPa | 15700 psi | |
Poco Graphite Glassmate® SR Graphite An economical material for short production runs. An ideal insert material for thick bead transfer applications. |