Polymer Property : Compressive Strength = 1.96 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 1.96 MPa
284 psi
Cold Crushing
Sharadaa Ceramics 0.5 Insulation Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 1.96 - 2.94 MPa
284 - 427 psi
Cold Crushing
Sharadaa Ceramics HF 60 AL Insulation Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 1.96 MPa
284 psi
Fired at 800°C, Cold Crushing
Sharadaa Ceramics REFINSUL ZAP-015 Insulating Castables
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l..
Compressive Strength 1.96 MPa
284 psi
Dried at 110°C, Cold Crushing
Sharadaa Ceramics REFINSUL ZAP-016 Insulating Castables
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l..