Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1.25 MPa | 181 psi | 30 g/l |
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be.. |