Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.981 - 1.47 MPa | 142 - 213 psi | Cold Crushing |
Sharadaa Ceramics CFI Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Compressive Strength | <= 0.981 MPa | <= 142 psi | Cold Crushing Strength |
Chosun Refractories A-7 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 0.981 MPa | <= 142 psi | Cold Crushing Strength |
Chosun Refractories LW-24 Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 0.981 MPa | <= 142 psi | Cold Crushing Strength |
Chosun Refractories LW-28 Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 0.981 MPa | <= 142 psi | Cold Crushing Strength |
Chosun Refractories A-6 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 0.981 MPa | 142 psi | Cold Crushing Strength |
Chosun Refractories CFA-1 Ceramic Foam Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 0.981 MPa | 142 psi | Cold Crush Strength |
BNZ Materials PA 23 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Compressive Strength | 0.981 MPa | 142 psi | Cold Crushing |
Sharadaa Ceramics 0.4 Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |