Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.641 MPa | 93.0 psi | Core; ASTM C365 |
3M RPF-CWR (0.417 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass with Woven Roving 3M™ RPF-C (Reinforced Polyurethane Foam) is a polyurethane foam with layers of continuous strand fiberglass and woven roving throughout the polyurethane. The composites are 30% to 45% lighter than .. |