Polymer Property : Compressive Strength = 0.0138 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.0138 - 0.0345 MPa
2.00 - 5.00 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ C121A Neoprene/SBR
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0138 - 0.0345 MPa
2.00 - 5.00 psi
Deflection @ 25%; ASTM D1056
Monmouth Rubber & Plastics Durafoamâ„¢ C41 Closed Cell Epichlorohydrin
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0138 - 0.0345 MPa
2.00 - 5.00 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ C41NBR Nitrile Rubber
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0138 - 0.0345 MPa
2.00 - 5.00 psi
Deflection @ 25%
Monmouth Rubber & Plastics Durafoamâ„¢ DK1111 NEO/EPDM Polymeric Blend
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0138 - 0.0345 MPa
2.00 - 5.00 psi
0.25; ASTM D1056
Monmouth Rubber & Plastics Durafoamâ„¢ IVN 41 NEO/PVC/NBR
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0138 - 0.0345 MPa
2.00 - 5.00 psi
Deflection @ 25%; ASTM D1056
Monmouth Rubber & Plastics Durafoamâ„¢ N231 100% Neoprene
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0138 - 0.0345 MPa
2.00 - 5.00 psi
Deflection @ 25%
Monmouth Rubber & Plastics Durafoamâ„¢ N231XS 100% Neoprene
Information provided by Monmouth Rubber & Plastics Corp.
Compressive Strength 0.0138 - 0.0345 MPa
2.00 - 5.00 psi
0.25
Monmouth Rubber & Plastics Durafoamâ„¢ P191HD EPDM
The Durafoam™100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ¼ inc..
Compressive Strength 0.0138 MPa
2.00 psi
10% deformation
Unifrax Isofrax® 1260C Paper Fiber
Isofrax® 1260C Paper is a unique product which is manufactured by forming Isofrax 1260C Fiber in a nonwoven matrix. The fibers are randomly oriented during manufacture, then held in place with a l..
Compressive Strength 0.0138 MPa
2.00 psi
ASTM D3574
3M 4714 Foam Tape
Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio..
Compressive Strength 0.0138 - 0.0345 MPa
2.00 - 5.00 psi
25% PSI Compression
Monmouth Rubber & Plastics Durafoam™ C19XLDS EPDM
Special Features: Extremely soft and conforms easily to irregular surfaces Superior buoyancy Excellent chemical resistance 100% free of HCFC & CFC Available in custom colors upon request for quoteCo..
Compressive Strength 0.0138 MPa
2.00 psi
Deflection, Compress 25%; ASTM D3574
3M 4714 Single-Coated Foam Tape
3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast..
Compressive Strength 0.0138 MPa
2.00 psi
ASTM D3574
3M 4718 Foam Tape
Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio..
Compressive Strength 0.0138 MPa
2.00 psi
Deflection, Compress 25%; ASTM D3574
3M 4718 Single-Coated Foam Tape
3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast..