Polymer Property : Tensile Strength = 5680 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 39.1 MPa
>= 5680 psi
ASTM D 638
Karina 822-18/599-CRB-LMP Gray PVC Compound
Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.1 MPa
>= 5680 psi
ASTM D 638
Karina E 822-10/148-CRB-LMP White PVC Compound
Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.1 MPa
>= 5680 psi
ASTM D 638
Karina E 854-35/1-A-ERYB Ivory PVC Compound
Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.1 MPa
>= 5680 psi
ASTM D 638
Karina E 854-35/1-Y-ERYB Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 39.1 MPa
>= 5680 psi
ASTM D 638
Karina E 857-35/1-A-ERYB Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.