Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 386 - 607 MPa | 56000 - 88000 psi | |
Chicago Extruded Metals BioBrass® UNS C46400 Copper-Zinc-Tin Alloy Copper-Zinc-Tin Alloy (Naval Brass)Finished product available as bar, wire, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, H04, M30Information provided by Chicago Extruded Met.. |
|||
Tensile Strength | 276 - 607 MPa | 40000 - 88000 psi | |
Chicago Extruded Metals UNS C34000 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar or rod.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |