Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 20.0 - 40.0 MPa | 2900 - 5800 psi | Compression; ISO 527 |
Raschig Group DECAL® 937 Phenolic Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W.. |
|||
Tensile Strength | 25.0 - 40.0 MPa | 3630 - 5800 psi | Compression; ISO 527 |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |
|||
Tensile Strength | 28.0 - 40.0 MPa | 4060 - 5800 psi | DIN 53455 |
Isoflon TFM Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Strength | 32.0 - 40.0 MPa | 4640 - 5800 psi | DIN 53455 |
Isoflon PCTFE Polychlorotrifluoroethylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Strength | 30.0 - 40.0 MPa | 4350 - 5800 psi | ISO 527 |
Bulk Molding Compounds tetra-DUR F 4206 Bulk Molding Compound General purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), ther.. |