Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 6.14 MPa | 890 psi | Silicone Property; ASTM D412 |
Arlon 51571B015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical.. |
|||
Tensile Strength | 6.14 MPa | 890 psi | Side 1, Silicone Property; ASTM D412 |
Arlon 51576B015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate.. |
|||
Tensile Strength | 6.14 MPa | 890 psi | Silicone Property; ASTM D412 |
Arlon 55572AA024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be us.. |
|||
Tensile Strength | 6.14 MPa | 890 psi | Side 1 Silicone Property; ASTM D412 |
Arlon 55576R060 0.060" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Tensile Strength | 6.14 MPa | 890 psi | Side 1 and Side 2, Layer 1; Compound Property; ASTM D412 |
Arlon 55578R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: LDPESide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Silicone Skim Coat Appearance: Red silico.. |
|||
Tensile Strength | 6.14 MPa | 890 psi | Side 1, Layer 1 and Side 2; Compound Property; ASTM D412 |
Arlon 55578R030 0.0325" (0.825 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1, Layer 2: Uncured Silicone Rubber Side 1, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Cured Silicone Rubber Appearance:.. |
|||
Tensile Strength | 6.14 MPa | 890 psi | Side 1 and Side 2, Layer 1; Compound Property; ASTM D412 |
Arlon 55578R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Appearance:.. |
|||
Tensile Strength | 6.14 MPa | 890 psi | Layer 2, Silicone Property; ASTM D412 |
Arlon 55579R031H 0.0315" (0.800 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: LDPELayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. T.. |
|||
Tensile Strength | 6.14 MPa | 890 psi | Layer 2, Silicone Property; ASTM D412 |
Arlon 55579R055 0.054" (1.37 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass clot.. |
|||
Tensile Strength | 6.14 MPa | 890 psi | Layer 1 Silicone Property; ASTM D412 |
Arlon 56579R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production mate.. |
|||
Tensile Strength | 6.14 MPa | 890 psi | Side 1, Silicone Property; ASTM D412 |
Arlon 51576R015D 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical v.. |
|||
Tensile Strength | 6.14 MPa | 890 psi | Side 1, Silicone Property; ASTM D412 |
Arlon 51576R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Tensile Strength | 6.14 MPa | 890 psi | Side 1, Silicone Property; ASTM D412 |
Arlon 51576W015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: White silicone gum on glass fabricThis data re.. |
|||
Tensile Strength | 6.14 MPa | 890 psi | Side 1, Compound; ASTM D412 |
Arlon R36133N062 0.062" (1.57 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production ma.. |