Mechanical Properties Metric English Comments
Tensile Strength 58.6 MPa
8500 psi
ASTM D638
Plaskolite Optix® CA-68 General Purpose Acrylic Resin
Injection Molding and Extrusion Grade. Good heat resistance, medium flow.
Tensile Strength 58.6 - 68.9 MPa
8500 - 10000 psi
ASTM D638
Mar-Bal MB2000-25 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Tensile Strength 58.6 MPa

@Thickness 3.18 mm
8500 psi

@Thickness 0.125 in
ASTM D638
Solvay Specialty Polymers Radel® R-7700 Polyphenylsulfone (PPSU)
Radel® R-7700 polyphenylsulfone sheet was developed specifically for aircraft interior applications. Through the use of a proprietary flame retardant package, this resin offers low heat release, ..
Tensile Strength 58.6 MPa
8500 psi
Master Bond EP36CLV One Component Heat Resistant Liquid Flexible Epoxy
Master Bond Polymer System EP36CLV is a one component, high temperature resistant, B staged epoxy that cures with excellent toughness and is far less rigid than typical high temperature resistant ep..
Tensile Strength >= 58.6 MPa
>= 8500 psi
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System
Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi..
Tensile Strength 58.6 MPa
8500 psi
ASTM D412
Lubrizol ESTANE® 54600 Ester Based Thermoplastic Polyurethane
Features: Very good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion Available in Americas, Europe,..
Tensile Strength 58.6 MPa
8500 psi
ASTM D638
Ensinger XP-150 Compression Molded Polyimide Unfilled, Premium Grade
The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal st..
Tensile Strength 58.6 - 72.4 MPa
8500 - 10500 psi
Bulk Molding Compounds BMC T15(GP) General Purpose Molding Compound
BMC T15(GP) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GP) is well suited for a variety of applications. It is av..
Tensile Strength 58.6 MPa
8500 psi
ASTM D638