Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 5.50 MPa | 798 psi | Solid Silicone Rubber Sheet |
P & P Technology Silicone Sheet Silicone sheet is FDA approved. Translucent sheet is FDA @ WRC approved. FDA Certificate No. 177.2600Information provided by P & P Technology |
|||
Tensile Strength | 5.50 MPa | 798 psi | |
Momentive Performance Materials Electro 170 Heat Cured Rubber - High Voltage Insulating Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 5.50 MPa @Strain 100 % |
798 psi @Strain 100 % |
ISO 37 |
BASF Elastollan 685 AU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 5.50 MPa | 798 psi | 100; ISO 37 |
BASF Elastollan SP 9213 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | >= 5.50 MPa | >= 798 psi | in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C70.250 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Tensile Strength | 5.50 MPa | 798 psi | 100; ISO 37 |
BASF Elastollan 880 AN TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 5.50 MPa | 798 psi | ISO 37 |
AlphaGary Evoprene™ 3273 Standard SBS Thermoplastic Elastomer Compound |
|||
Tensile Strength | 5.50 MPa | 798 psi | ISO 37 |
AlphaGary Evoprene™ 003 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tensile Strength | 5.50 MPa | 798 psi | ISO 37 |
AlphaGary Evoprene™ Super G 947 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |