Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 4.83 MPa @Strain 100 % |
701 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible D7500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 4.83 MPa @Strain 100 % |
701 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible D8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 4.83 MPa @Strain 100 % |
701 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3684 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength | 4.83 MPa @Strain 100 % |
701 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C7500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 4.83 MPa @Strain 100 % |
701 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C75A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 4.83 MPa | 701 psi | Transverse Direction, typical properties Injection molded plaques, Die C; ASTM D412 |
Kraton® D2109 DS-N (SBS) Compound Description: Kraton D2109 DS-N is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Tensile Strength | 4.83 MPa | 701 psi | Transverse Direction, typical properties Injection molded plaques, Die C; ASTM D412 |
Kraton® D2109 DS-W (SBS) Compound Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |