Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 46.02 MPa | 6674 psi | ASTM D638 |
I. Stern 750 Medium Impact Black ABS Features:Easy color-abilityInjection MoldingApplicationsOffice equipmentElectronic partsSpools, ReelsInformation provided by I. Stern & Co. Inc. |