Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 4.30 MPa | 624 psi | |
Shin-Etsu Silicones KE-1830 Silicone, RTV Adhesive/Sealant Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 4.30 MPa | 624 psi | ASTM D 638 |
API Megol AM DP2433/50PBT SEBS Adhesion Modified Overmolding for Polyesters Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |