Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E-844-10/219-Y-ERYM White PVC Compound Tin stabilized PVC compound, recommended for extrusion of profiles for general applications. It is supplied in pellet form and should be processed at the temperature range of 170°C to 190°C.I.. |
|||
Tensile Strength | 39.2 MPa | 5690 psi | ASTM D412 |
Kolon ELLAS K-475A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionIndustry PartsParts for Automobile/Mobile phoneInformation provided by API-Kolon. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 803-36/9-AY-ERYB Brown PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 805-10/152-A-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 806-10/42-B-RT-PO White PVC Compound PVC powder compound, recommended for extrusion in twin screw extruder of sewer pipes.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 806-18/364-BY-ERYB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 806-48/1-BY-ERYB Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 810-37/3-CRB Ocher PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 811-10/23-A-ERYB-PO White PVC Compound PVC powder compound, recommended for extrusion in twin screw extruder of sewer pipes.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | NBR NM-IEC 60811-1-1 |
Karina 828-08/20-AY-ERYB Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 828-08/20-AY-ERYB-PO Beige PVC Compound PVC powder compound recommended for extrusion in twin screw extruder of door profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 830-48/1-AY-ERYB Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 834-48/1-A-ERM-LMP Black PVC Compound Heavy metal free PVC compound recommended for extrusion of automotive profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 837-35/1-A-ERYB-LMP Ivory PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 76/205-IS-SD-TR Crystal PVC Compound Crystal PVC compound recommended for sleeves.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 76/205-IS-SD-TR Crystal PVC Compound Crystal PVC compound recommended for sleeves.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 800-18/695-CY-RT-PO Compound PVC Gray Rigid PVC compound dry blend, recommended for extrusion of discharge pipes/tubes.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 800-35/1-B-ERB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 813-10/164-B-RT-PO White PVC Compound PVC powder compound, recommended for extrusion in twin screw extruder of sewer pipes.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 828-08/497-Y-RT Beige PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 828-18/569-Y-RT Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 828-48/27-Y-RT Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 833-10/84-Y-ERYM White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 835-10/155-C-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 835-18/115-C-ERYB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 39.2 MPa | 5690 psi | 50 mm/min; ISO 527-1,-2 |
Gromax ATE90-FN01N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | 39.2 MPa | 5690 psi | |
Taiwan Sheen Soon Sheenthane® A8870E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 39.2 MPa | 5690 psi | |
Taiwan Sheen Soon Sheenthane® A8871E2 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 802-10/93-AY-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 842-18/106-Y-RT-POWDER Compound PVC Gray Rigid powder PVC compound recommended for extrusion of profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |