Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 270 MPa @Temperature -35.0 °C |
39200 psi @Temperature -31.0 °F |
Typical |
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual .. |