Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 26.0 MPa | 3770 psi | ISO 527 |
Murtfeldt Original Material ”S”® plus + FP Polyethylene Original Material ”S”® plus+ FP [FS] is a technical plastic that completely meets the requirements of the food sector for the detectability of plastic foreign bodies in foods. “FP” stands for “.. |
|||
Tensile Strength | 26.0 MPa | 3770 psi | ASTM D412 |
S&E Specialty Polymers GA-1046-80E PVC Application: A high-grade 80° C semi-rigid PVC insulation compound.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 26.0 MPa | 3770 psi | ASTM D638 |
Premix Premi-Ject® 1102H Fiberglass Reinforced Thermoset BMC Premi-Ject® 1102H is a fiberglass reinforced thermoset bulk molding compound for coil encapsulation applications.Key features and benefits are:Designed with unique flow properties to encapsulate co.. |
|||
Tensile Strength | 26.0 MPa | 3770 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 7140 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 7140 is a static dissipative thermoplastic masterbatch based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 7140 has been developed for.. |
|||
Tensile Strength | 26.0 MPa | 3770 psi | |
Imerys ImerPlast™ 10WPC Recycled Polyolefin Resin ImerPlast 10WPC is a black, UV stabilized, recycled resin with no significant odor, for compounding with wood flour for extruded decking applications. Melt filtered to 250 µm to ensure no particu.. |
|||
Tensile Strength | 26.0 MPa | 3770 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-2185 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 26.0 MPa | 3770 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8185 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 26.0 MPa @Strain 300 % |
3770 psi @Strain 300 % |
ISO 37 |
BASF Elastollan C 98 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 26.0 MPa | 3770 psi | ISO 37 |
BASF Elastollan SP 9213 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 26.0 MPa | 3770 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1580 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 26.00 MPa | 3770 psi | ASTM D882 |
E-Polymers EFLEX® I1020 Ionomer I-series (Ionomer): E-FLEX Ionomer is a family of ethylene acrylic acid (E/AA) copolymers, in which part of the acrylic acid is neutralized with metal ions such as zinc (Zn) or sodium (Na) or magnes.. |