Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 24.8 MPa | 3600 psi | ASTM D638 |
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Tensile Strength | 24.8 MPa | 3600 psi | ASTM D412 |
Northstar Polymers MPG-D70A Room-Temperature-Curable Polyurethane Casting Elastomer MPG-D70A is room-temperature-curable polyurethane casting elastomer system designed for molding polyurethane parts with tough, but flexible physical characteristics. The typical applications for th.. |
|||
Tensile Strength | 24.8 MPa | 3600 psi | ASTM D638 |
I. Stern HIPS 8 High Impact Polystyrene Injection Grade Features:Good processing characteristicsComplies with FDA requirements as described in Title 21 CFR 177.1640ApplicationsDisplaysHouse waresStructural FoamInformation provided by I. Stern & Co. Inc. |
|||
Tensile Strength | 24.8 MPa | 3600 psi | |
Lucite International Elvacite ® 2045 Acrylic Resin Elvacite® 2045 is a high molecular weight iso-butyl methacrylate polymer. Elvacite® 2045 is useful in topcoats for vacuum metallized plastics and in lacquers for other solvent – sensitive.. |
|||
Tensile Strength | 24.8 MPa | 3600 psi | 2 in/min; ASTM D638 |
Braskem TI4130G Impact Copolymer Polypropylene Description: Medium izod impact, good blush resistance, good low temperature drop impact.Applications: Suggested uses include furniture, housewares, automotive interior trim. UL temperature index of.. |
|||
Tensile Strength | 24.8 MPa | 3600 psi | ASTM D638 |
Americas Styrenics STYRON® 487R High Impact Polystyrene Product CharacteristicsToughnessHeat resistanceGood stiffnessFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by Amer.. |