Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 216 MPa | 31300 psi | RT; ASTM D638 |
Rogers Corporation XT/duroid™ 8100 0.002" Woven Glass Reinforced Thermoplastic Circuit Material XT/duroid™ 8100 woven glass reinforced thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 81.. |
|||
Tensile Strength | 216 MPa | 31300 psi | ASTM D638 |
Kolon KOPA® KN333G45 G/F Reinforced Nylon 66 G/F 45% reinforcedApplications Internal gearsInformation provided by API-Kolon. |
|||
Tensile Strength | 216 MPa | 31300 psi | ASTM D638 |
E-Polymers TEKAMID® TA250G60 60% Glass Fiber Reinforced, High Modulus PA66 Resin Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,.. |