Mechanical Properties Metric English Comments
Tensile Strength 186.39 MPa
27034 psi
ASTM D638
E-Polymers SEPAZ® V230A 30% Glass Fiber Reinforced PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..