Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1790 MPa | 260000 psi | 52 HRC |
Schmolz + Bickenbach Thermodur® 2344 Magnum Hot Work Die Steel Description: Thermodur® 2344 Magnum is an electro slag remelted (ESR) hot work die steel, designed to meet all die casting industry specificationCharacteristics: Excellent toughness; Excellent re.. |