Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 17.0 MPa | 2470 psi | ISO 527 |
S&E Specialty Polymers TufFill™ 5008 Polyolefin Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV p.. |
|||
Tensile Strength | 17.0 MPa | 2470 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o.. |
|||
Tensile Strength | >= 17.0 MPa | >= 2470 psi | DIN 53504 |
NEXA® PFX9020 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
Tensile Strength | 17.0 MPa | 2470 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Tensile Strength | 17.0 MPa | 2470 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP TIVAR® SuperPlus PE-UHMW + specific additives (ISO Data) TIVAR SuperPlus is a wear optimised, partially cross-linked PE-UHMW material with extremely high degree of polymerisation for use in most demanding applications and environments. When used for drain.. |
|||
Tensile Strength | 17.0 MPa | 2470 psi | ASTM D2095 |
Permabond UV610 UV-curable Adhesive PERMABOND UV610 is a single part, fast setting, UV curable adhesive designed specifically for bonding glass and metal. Its high strength makes it suitable for a wide range of applications including .. |
|||
Tensile Strength | 17.0 MPa @Strain 100 % |
2470 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2190G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2190G is a 90 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2190G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Tensile Strength | 17.0 - 22.0 MPa | 2470 - 3190 psi | ASTM D4894 |
Isoflon PTFE + 60% Bronze Polytetrafluoroethylene with 60% Bronze Properties:Excellent wear and compression resistance (low cold creep)Good thermal conductivityImproved coefficient of friction when combined with Mos² or graphiteApplications: Dynamic seals for .. |
|||
Tensile Strength | 17.0 - 23.0 MPa | 2470 - 3340 psi | molded; ASTM D4745 |
Guarniflon PTFE G420 Polytetrafluoroethylene 50% Steel PTFE G Special Compound with steelInformation provided by Guarniflon® |
|||
Tensile Strength | 17.0 MPa | 2470 psi | ASTM D412 |
Dynasol Solprene® 4302 Thermoplastic Rubber (SBS) Solprene 4302 is a linear block copolymer of styrene and butadiene, having 31% styrene content, most of it forming a polystyrene block, which gives the polymer a thermoplastic behavior. It has a non.. |
|||
Tensile Strength | 17.0 MPa @Strain 20.0 % |
2470 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan B 64 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 17.0 MPa @Strain 100 % |
2470 psi @Strain 100 % |
ISO 37 |
BASF Elastollan C 59 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 17.0 - 24.0 MPa | 2470 - 3480 psi | molded; ASTM D4894, ASTM D4745 |
Guarniflon PTFE G403 Polytetrafluoroethylene 15% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |
|||
Tensile Strength | 17.0 - 23.0 MPa | 2470 - 3340 psi | molded; ASTM D4894, ASTM D4745 |
Guarniflon PTFE G458 Polytetrafluoroethylene 60% Bronze, 2% Carbon PTFE G Standard Compound with bronzeProperties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.Application: Unlubricated bearings for high speed excluding hard .. |