Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 15.7 MPa | 2280 psi | Dry Heat Aging 392°F; 70 hr; ASTM D865 |
Seals Eastern 7346 Extreme Low Temperature Service Rubber HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern. |
|||
Tensile Strength | 15.7 MPa | 2280 psi | 20 in/min; ASTM D638 |
Teknor Apex Sinvicomp SHE 8500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength | 15.7 MPa | 2280 psi | 20 in/min; ASTM D638 |
Teknor Apex Sinvicomp SME 6100 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength | 15.7 MPa | 2280 psi | 20 in/min; ASTM D638 |
Teknor Apex Sinvicomp SME 6330A Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex |