Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 15.59 MPa @Treatment Temp. 136 °C, Time 605000 sec |
2261 psi @Treatment Temp. 277 °F, Time 168 hour |
Oven aged |
S&E Specialty Polymers GA-509ORLT PVC Application: Lead free, flame retardant UV and oil resistant PVC jacketing compound with superior low temperature properties.Information provided by S&E Specialty Polymers |