Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1.50 MPa | 218 psi | ASTM D412 |
P & P Technology EC-H Silver Copper Loaded Fluorosilicone P & P Technology material reference EC-H is a printing grade fluorosilicone elastomer with a Silver/Copper conductive filler and is green in color. The material is specially compounded to offer exc.. |
|||
Tensile Strength | 1.50 MPa | 218 psi | |
Shin-Etsu Silicones KE-3493 Silicone, RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 1.50 MPa @Strain 20.0 % |
218 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan C 65 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 1.50 MPa | 218 psi | average; perpendicular to plane; ASTM C297 |
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |
|||
Tensile Strength | >= 1.50 MPa | >= 218 psi | perpendicular to plane; ASTM C297 |
3A Composites Core Materials AIREX® T92.100 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |
|||
Tensile Strength | 1.50 MPa @Strain 20.0 % |
218 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan C 70 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 1.50 MPa | 218 psi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C71.55 Elevated Temperature Structural Foam AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength.. |