Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 135 MPa | 19600 psi | ASTM D638 |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP), 30% Glass Fiber Xydar® G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology.The moldab.. |
|||
Tensile Strength | 135 MPa | 19600 psi | 5 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226F3 Nylon 6.6, 15% Glass Fiber SAXAMID 226F3 is a polyamide 6.6 injection-molding-grade reinforced with 15% glass fibers. This grade is suitable for applications requiring high strength and very good flow properties during proces.. |
|||
Tensile Strength | 135 MPa @Thickness >=1.50 mm |
19600 psi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6 |
Elektro-Isola Etronax P EP Phenolic, Polyester Fabric Reinforcement, Light Yellow, Sheets Description: This material is exceptionally strong and tough. Very low water absorption and the lowest swelling in water. High resistance to chemicals, including SF6 gas. Applications: Can be used i.. |
|||
Tensile Strength | >= 135 MPa | >= 19600 psi | IEC 1212-2 5.7 |
Hippe EP PC 301 Woven Polyester Cloth Reinforced Epoxy Resin - Sheet Used in electrical and mechanical applications. Good resistance to SF6.Information provided by Hippe. |
|||
Tensile Strength | 135 MPa | 19600 psi | ASTM D638 |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP)
(Unverified Data**) Xydar G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology. The moldabili.. |