Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 13.45 MPa @Treatment Temp. 100 °C, Time 346000 sec |
1951 psi @Treatment Temp. 212 °F, Time 96.0 hour |
ATM Oil #2 |
S&E Specialty Polymers GTPE-2272ALC PVC Application: Flame retardant, matt finish, 90° C, flexible, oil resistant, TPE jacketing material.Information provided by S&E Specialty Polymers |