Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 11.6 MPa | 1680 psi | ASTM D638 |
S&E Specialty Polymers G-4275E Application: General-purpose extrusion material designed for profile extrusion applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 11.6 MPa @Strain 100 % |
1680 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3870 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength | 11.6 MPa | 1680 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4985F Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Tensile Strength | 11.6 - 13.3 MPa | 1680 - 1930 psi | ASTM D 638 |
API Megol AM SV/P SEBS Adhesion Modified Overmolding for Polar Polymers Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |