Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 10.9 MPa | 1580 psi | ASTM D412 |
S&E Specialty Polymers GE-960F PVC Description: Matte finish, expandable oil resistant flexible PVC/Nitrile alloyInformation provided by S&E Specialty Polymers |
|||
Tensile Strength | 10.9 MPa @Strain 100 % |
1580 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength | 10.9 MPa @Strain 100 % |
1580 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A9001 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength | 10.9 MPa @Strain 100 % |
1580 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A90U2 Polyvinyl Chloride, Flexible (PVC, Flexible) GENERAL PURPOSE CLEAR PVC COMPOUND WITH LOW LEVEL OF U.V. INHIBITOR, to be used only in interior applications.Information provided by PolyOne |
|||
Tensile Strength | 10.9 MPa | 1580 psi | NF T 46-002 |
SMAC SMACTANE® SP Damping Material A viscoelastic rubber material developed by SMAC for space applications and maximizes the damping properties in a wide range of temperatures & frequencies Damping properties: Damping properties are .. |