Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 102 MPa | 14800 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Techtron® PPS unfilled, extruded (ISO Data) This unfilled polyphenylene sulfide based material is ideal for structural applications in corrosive environments or as a PEEK replacement at less demanding temperatures. Very good dimensional stabi.. |
|||
Tensile Strength | 102 MPa | 14800 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over a b.. |
|||
Tensile Strength | 102 MPa | 14800 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA), 22% Mineral Amodel® A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over.. |
|||
Tensile Strength | 102 MPa | 14800 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 102 MPa | 14800 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 102 MPa @Strain 8.00 %, Temperature 0.000 °C |
14800 psi @Strain 8.00 %, Temperature 32.0 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 3000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 102 MPa | 14800 psi | ASTM D638 |
Aaron Industries AAROPRENE® GFN 6613 Glass Filled Nylon 6/6 AAROPRENE® GFN & MFN 6600 Series Reinforced CompoundsColor may be specified. |
|||
Tensile Strength | 102.0 MPa | 14800 psi | ASTM D638 |
E-Polymers SEPAZ® N2020L Nanoclay 2% High flow Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |