Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1.00 MPa | 145 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 7005 High Clarity Liquid Silicone Rubber This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 1.00 MPa | 145 psi | |
Sawbones Solid Rigid Polyurethane Foam 5 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
Tensile Strength | 1.00 MPa | 145 psi | ISO 1798 |
Zotefoams ZOTEK® F OSU Rigid PVDF Foam Zotek® F OSU is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and .. |
|||
Tensile Strength | 1.00 MPa @Strain 20.0 % |
145 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan B 60 A ESD TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 1.00 MPa @Strain 20.0 % |
145 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan S 60 A SPF TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 1.00 MPa | 145 psi | 20; ISO 37 |
BASF Elastollan 2180 A TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 1.00 MPa @Strain 20.0 % |
145 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan 670 AWHU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 1.00 MPa | 145 psi | ASTM D 412 |
Eurofoam Porocell POR 302/T-E NBR/PVC Foam Acrylonitrile butadiene and polyvinyl chloride foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurof.. |
|||
Tensile Strength | 1.00 MPa @Strain 20.0 % |
145 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan S 60 AWH TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | >= 1.00 MPa | >= 145 psi | in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C70.55 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Tensile Strength | >= 1.00 MPa | >= 145 psi | in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C71.55 Elevated Temperature Structural Foam AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength.. |
|||
Tensile Strength | 1.00 MPa @Strain 20.0 % |
145 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan B 60 A WHA TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |