Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 9.60 MPa | 1390 psi | |
Momentive Performance Materials TUFELâ„¢ II 94405 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 9.60 MPa | 1390 psi | |
Momentive Performance Materials TUFELâ„¢ II 94406 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 9.58 MPa | 1390 psi | |
Shin-Etsu Silicones FE-273U Elastomer FE-273U is high modulus and low compression set fluorosilicone compounds. It is designed to process well in modling application.FeaturesExcellent fuel and solvent resistanceUsable over a broad temp.. |
|||
Tensile Strength | 9.60 MPa | 1390 psi | |
Shin-Etsu Silicones LIMSâ„¢ KEG2000-40A/B Elastomer KEG2000-40 is a fast cure type liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to.. |