Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 8.27 MPa @Strain 100 % |
1200 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A85UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 8.27 MPa @Strain 100 % |
1200 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 8.27 MPa @Strain 100 % |
1200 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B85B0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 8.27 MPa @Strain 100 % |
1200 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B87FB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 8.27 MPa @Strain 100 % |
1200 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV 3450 Polyvinyl Chloride, Flexible (PVC, Flexible) NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of.. |
|||
Tensile Strength | 8.27 MPa @Strain 100 % |
1200 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3881 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 8.27 MPa | 1200 psi | ASTM D412 |
Arlon 10502N080 0.080" (2.3 mm) Cured Silicone Rubber (Unsupported)
(discontinued **) Vacuum Bag SubstrateDesign/Construction:Interleave: PolyethyleneMaterial: Cured Silicone RubberAppearance: Translucent silicone rubberThis data represents typical values for the production material... |
|||
Tensile Strength | 8.27 MPa | 1200 psi | Typical |
Garlock 363 Nitrile Sheet Rubber Nitrile sheet is primarily used for applications where resistance to oil, solvents and fuels is required.Style #363 is a good quality, oil-resistant nitrile sheet.Information provided by Garlock Rub.. |
|||
Tensile Strength | >= 8.27 MPa | >= 1200 psi | |
Garlock 4160 Natural Sheet Rubber Excellent general purpose gasket materials for air, hot and cold water, saturated steam and exterior service.Red, smooth finishInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | 8.27 MPa | 1200 psi | Typical |
Garlock 567 EPDM Sheet Rubber Excellent general purpose gasket materials for air, hot and cold water, saturated steam and exterior service.Black, smooth finish, commercial qualityInformation provided by Garlock Rubber Technologi.. |
|||
Tensile Strength | 8.27 MPa | 1200 psi | ASTM F152 |
Garlock 9780 Fluoroelastomer Sheet Rubber Gasketing Proprietary blend of fluoroelastomer.Resistant to severe chemicals and steam.Information provided by Garlock Rubber Technologies |
|||
Tensile Strength | 8.27 MPa | 1200 psi | ASTM F152 |
Garlock THERMA-PURâ„¢ 4122-CMG High Temperature Gasketing Material THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a u.. |
|||
Tensile Strength | 8.27 MPa | 1200 psi | ASTM F152 |
Garlock THERMA-PURâ„¢ 4122-KAMM High Temperature Gasketing Material THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a u.. |
|||
Tensile Strength | 8.27 MPa | 1200 psi | Typical properties on film cast from toluene solution; ASTM D412 |
Kraton® D1117 P (SIS) Linear Triblock Copolymer Description: Kraton D1117 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 17%. It is supplied from North America in the physical form identified: .. |
|||
Tensile Strength | 8.30 MPa | 1200 psi | Flatwise |
Henkel Hysol EA 9695 Film Adhesive Second generation, low flow, composite bonding film; excellent environmental resistance. Composite structure repair, cure and co-cure with composite laminates. Qualified to Airbus. Data from .050 ps.. |
|||
Tensile Strength | 8.30 MPa | 1200 psi | |
Momentive Performance Materials FSE7540 Heat Cured Fluorosilicone Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 8.27 MPa | 1200 psi | ASTM D638 |
Saint-Gobain Rulon® F Grade Bearing/Seal PTFE F Grade Bearing/Seal PTFE is used for applications requiring a long wearing material, especially in dry applications and those requiring high abrasion resistance. Standard tape liner material for Ru.. |
|||
Tensile Strength | 8.30 MPa | 1200 psi | |
Shin-Etsu Silicones LIMSâ„¢ KE2095-60AB Elastomer KE-2095-60 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Tensile Strength | 8.27 MPa | 1200 psi | |
Teknor Apex Tekbond® TB 1416A Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Tensile Strength | 8.27 MPa | 1200 psi | |
Teknor Apex Tekbond® TB 2183R1 Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Tensile Strength | 8.27 MPa | 1200 psi | Silicone Property; ASTM D412 |
Arlon HSLW301R##-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: High Strength, 1 inch wide, 30 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicate.. |
|||
Tensile Strength | 8.27 MPa | 1200 psi | Silicone Property; ASTM D412 |
Arlon LW401A##-P3 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Blue, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length .. |
|||
Tensile Strength | 8.27 MPa | 1200 psi | Silicone Property; ASTM D412 |
Arlon R34581R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 7628 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents ty.. |
|||
Tensile Strength | 8.27 MPa | 1200 psi | Silicone Property; ASTM D412 |
Arlon R34591R014 0.014" (0.356 mm) Uncured Silicone Rubber Design/Construction:Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 2116 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Appearance: Red silicon.. |
|||
Tensile Strength | 8.27 MPa | 1200 psi | |
AlphaGary AlphaSeal™ 04-073 P Modified Thermoplastic Elastomer AlphaSeal™ 04-073 P Modified is a TPE based material recommended for injection molded corks. AlphaSeal is formulated for low taste and low odor and exhibits good elastic recovery, abrasion resista.. |
|||
Tensile Strength | 8.27 MPa | 1200 psi | Silicone Property; ASTM D412 |
Arlon 54331R014 0.014" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: Blue LDPESide 1: Uncured Silicone RubberSubstrate: Style 2116 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Blue LDPEThis data represents typical valu.. |
|||
Tensile Strength | >= 8.27 MPa | >= 1200 psi | Compound Property |
Arlon R34880T020 0.020" (0.508 mm) Uncatalyzed, Unsupported rubber on a Mylar Carrier Design/Construction:Side 1: Uncatalyzed, Unsupported rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
Tensile Strength | 8.27 MPa | 1200 psi | ASTM D412 |
Arlon SFT 0.012" (0.305 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: PET Product: Cured Self-Fusing Silicone Rubber Cross-Section: 1” Wide RectangularDescription: 1 inch wide, 12 mil thick x 10 yards long, Gray, Rectangular cross-sec.. |
|||
Tensile Strength | 8.27 MPa @Strain 100 % |
1200 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3906 Polyvinyl Chloride, Flexible (PVC, Flexible) NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of.. |
|||
Tensile Strength | 8.27 MPa | 1200 psi | ASTM F152 |
Garlock THERMA-PUR™ 4122-FC High Temperature Gasketing Material THERMa-PUR™ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a uniqu.. |