Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 8.10 MPa

@Strain 100 %
1170 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R295AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 8.07 MPa

@Strain 100 %
1170 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible XV3844 Polyvinyl Chloride, Flexible (PVC, Flexible)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
Tensile Strength 8.10 MPa
1170 psi
Shin-Etsu Silicones LIMSâ„¢ KE2095-40AB Elastomer
KE-2095-40 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo..
Tensile Strength 8.07 MPa
1170 psi
Silicone Property; ASTM D412
Arlon 55173R045 0.045" (1.14 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Product Use: Press PadAppearance: Red silicone rubber on f..
Tensile Strength 8.07 MPa
1170 psi
Silicone Property; ASTM D412
Arlon 51808R011 0.011" (0.279 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Wash Coat This data represents typical values for the production ..
Tensile Strength 8.07 MPa
1170 psi
Silicone Property; ASTM D412
Arlon 55173R062 0.0622" (1.58 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Product Use: Press PadAppearance: Red silicone rubber on f..