Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 7.72 MPa @Strain 100 % |
1120 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3816 Polyvinyl Chloride, Flexible (PVC, Flexible) NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of.. |
|||
Tensile Strength | 7.70 MPa | 1120 psi | |
Momentive Performance Materials FSE7520 Heat Cured Fluorosilicone Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 7.72 MPa | 1120 psi | Typical properties on film cast from toluene solution; ASTM D412 |
Kraton® D1126 P (SIS) Radial Copolymer Description: Kraton D1126 P is a clear, radial copolymer based on styrene and isoprene, with a polystyrene content of 21%. In addition, it has a diblock content of 30% and high melt flow. It is supp.. |
|||
Tensile Strength | 7.70 MPa | 1120 psi | |
Shin-Etsu Silicones LIMSâ„¢ KE2090-70AB Elastomer KE-2090-70 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Tensile Strength | 7.70 MPa | 1120 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 2865PE Thermoplastic Elastomer Elastocon® 2865PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2865PE is FDA compliant and well suited for.. |
|||
Tensile Strength | 7.70 MPa | 1120 psi | 300; ISO 37 |
BASF Elastoblend LP 9192 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 7.70 MPa | 1120 psi | ISO 37 |
AlphaGary Evoprene™ Super G 949 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |