Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 7.50 MPa | 1090 psi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C70.250 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Tensile Strength | 7.50 MPa @Strain 300 % |
1090 psi @Strain 300 % |
ISO 37 |
BASF Elastollan C 75 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |