Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 77.9 - 91.7 MPa | 11300 - 13300 psi | |
Bulk Molding Compounds BMC T45HT Automotive Grade Molding compound BMC T45HT was designed for the very demanding applications of automotive under hood engine covers. It meets the GMP UP .007 specification for automotive under hood. BMC T45HT is a vinyl ester base.. |